Chinese
-Chinese
-English
English/Chinese
Products
Products
Aluminum surface treatment agent series
Cleaning agent series
Paint stripping and plating series
Electroplating additive series
Antique dyeing series

Normal temperature

 Home > Products > Normal temperature

Antique dyeing process
Copper black
Aluminum black
Tin black
Titanium black
Iron black
Stainless steel black
Nickel black
Zinc black
Silver black
Dehydrated antirust oil
Copper anti-tarnish
Copper chemical polishing agent
Imitation gold
Rubbing copper water
Coarsening agent

CWF-80395 Iron black

Iron black

Designed for blackening steel, it combines blackening and phosphating, thus greatly enhancing film adhesion and corrosion resistance.

  • Other parameters
  • Manual download

Using parameters

Concentration: 1:4-5

Temperature: normal temperature

PH: 1

Specific gravity: 7 grass green liquid